冷应用
良好的可成形性
无干燥或硬化时间
较强的抗冲击性
适应大小不等的管径
可在较宽温度范围内施工
项目 | T 5030-12 | T 5050-20 | 测试方法 | |
总厚度 | 0.30mm (11.81mils) | 0.50mm (19.69mils) | ASTM D1000 | |
聚氯乙烯薄膜厚度 | 0.20mm (7.87mils) | 0.40mm (15.75mils) | ASTM D1000 | |
胶粘剂层厚度 | 0.10mm (3.94mils) | 0.14mm (5.51mils) | ASTM D1000 | |
断裂伸长率 23°C (73.4°F) | 250% | 220% | ASTM D1000 | |
抗拉强度 23°C (73.4°F) | 45.0N/cm (25.7 lbs/in) | 70.5N/cm (40lbs/in) | ASTM D1000 | |
对钢的附着力 | 12°C (54°F) | 5.30N/cm (38.4oz/in) | 6.50N/cm (59.4oz/in) | ASTM D1000 |
23°C (73.4°F) | 4.50N/cm (41.1oz/in) | 5.30N/cm (38.4oz/in) | ||
70°C (158°F) | 0.43N/cm (3.9oz/in) | 0.50N/cm (4.6oz/in) | ||
PE/PVC的剥离强度 | 12°C (54°F) | 5.00N/cm (45.7oz/in) | 6.30N/cm (57.6oz/in) | ASTM D1000 |
23°C (74.4°F) | 4.00N/cm (36.5oz/in) | 5.30N/cm (48.4oz/in) | ||
70°C (158°F) | 0.42N/cm (3.8oz/in) | 0.55N/cm (5.2oz/in) | ||
冲击强度 | 14 J (123.91in.lbf) | 16 J (141.61in.lbf) | ASTM G14 | |
绝缘强度 | 20kv | 25kv | ASTM D149 | |
水蒸气透过率 | 0.15g/m2/24h.@23°C (73.4°F) | ASTM E96 | ||
吸水率 | 0.08% 24h.@23°C (73.4°F) | ASTM D570 | ||
常规应用 | -12 ºC to +70°C (+10°F to 158°F) | |||
常规服务 | -48°C to 85°C (-55°F to 185°F) | |||
操作温度 | 70°C (158°F) | |||
内芯直径 | 41 or 76mm (1.614 or 2.992in) | |||
卷材尺寸(宽度*长度) | 50 to 400mm X 15 to 120m (1.97 to 15.75in X 49.21 to 399.7ft) | |||
颜色 | 黑色/白色/蓝色 | |||
本产品应储存在干燥通风处,运输过程中必须保持相同环境。储存温度范围不得高于16°C (60°F),且不得高于49°C(120°F),湿度不高于90%。直立叠高≤5层。保质期限12个月。
通用要求:待涂覆区域必须保持清洁干燥,无油脂、油污及灰尘。
防止水汽凝结:施工前及施工期间,作业面温度必须始终高于露点温度3°C(37.4°F)或更高。
应用前检查:对作业表面存在的缺陷进行补救处理。
1、采取螺旋缠绕方式进行施工。
聚氯乙烯外包装应张紧通常重叠50%。最小25 毫米( 1 英寸)的重叠, 首次和终止缠绕应为直线环形缠绕。整个使用过程加足够的张力,以提供胶带的连续粘合。
2、根据NACE SP0274《电火花检测》标准,执行测试验收
1、整体涂层系统的物体不得承受来自支撑物或起重设备等的外力载荷。可选择非粘结外包材料进行增强防护,如:无纺聚丙烯毯等。
2、埋地回填时应保持洁净,不得含有可能损坏涂层系统的任何异物。